CILLOLIN AL 2812

smooth surface, styling faces

low heat transport
CILLOLIN AL 285
medium heat transport
CILLOLIN AL 2812
high heat transport
CILLOLIN AL 223
coarse surface, contour surfaces
low heat transport
CILLOLIN AL 285 G
medium heat transport
CILLOLIN AL 2812 G
high heat transport
CILLOLIN AL 223 G
Very coarse surface, demanding casting symmetry
low heat transport
CILLOLIN AL 285 GN
medium heat transport
CILLOLIN AL 3500 G
high heat transport
CILLOLIN AL 223 GD
very smooth casting face, low thermal conductivity
CILLOLIN AL 286
ascension pipes, tools, protectice pipes
PYRONOL
gravity dies and gate stones in vertical continuous casting
CILLOLIN AL 225
sliding properties (pinholes)
CILLOLIN AL 160
Ceramic runners (alcohol-based)
CILLOLIN AL 500
Sand moulds for magnesium casting
CILLOLIN MG 785

CILLOLIN AL 2812 eignet sich zur Anwendung auf Stahl- und Graugusskokillen im Al-Niederdruckkokillenguss und Schwerkraftguss.

 

CILLOLIN AL 2812

  • mittlerer Wärmetransport (halbisolierend)
  • reduziert die Ausfallzeiten durch Putzarbeiten und Neuschlichtung
  • erhöht die Produktivität
  • erzeugt eine gleichmäßige Oberflächenstruktur des Gussteils und vermeidet Kaltschweißstellen
  • vermeidet zu schnelles Absetzen durch hoch wirksame Thixotropierungsmittel
  • bietet optimale Haftung, insbesondere an den beweglichen Kokillenteilen
  • garantiert höchste Maßhaltigkeit der Gussstücke
  • erleichtert das schonende Herauslösen der fertigen Gussstücke aus der Kokille
  • in der Reihenfolge AL 2812 – AL 2812 G – AL 3500 G verbessertes Fließvermögen der Schmelze bei tendenziell zunehmender Rautiefe der Gussoberfläche

 

Aussehen: rötlich, pastöse Form

Geruch: neutral

Reaktionstemperatur: mind. 150°C, max. 300°C